The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 11, 2025

Filed:

Apr. 07, 2021
Applicant:

Lam Research Corporation, Fremont, CA (US);

Inventors:

Justin Oberst, Beaverton, OR (US);

Bryan L. Buckalew, Tualatin, OR (US);

Kari Thorkelsson, Santa Clara, CA (US);

Assignee:

Lam Research Corporation, Fremont, CA (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C25D 17/00 (2006.01); C25D 5/02 (2006.01); C25D 5/12 (2006.01); C25D 7/12 (2006.01); C25D 21/12 (2006.01); H01L 21/288 (2006.01);
U.S. Cl.
CPC ...
C25D 17/004 (2013.01); C25D 5/022 (2013.01); C25D 5/12 (2013.01); C25D 7/123 (2013.01); C25D 17/001 (2013.01); C25D 21/12 (2013.01); H01L 21/288 (2013.01);
Abstract

Sequential electrodeposition of metals into through-mask features on a semiconductor substrate is conducted such as to reduce the deleterious consequences of lipseal's pressure onto the mask material. In a first electroplating step, a first metal (e.g., nickel) is electrodeposited using a lipseal that has an innermost point of contact with the semiconductor substrate at a first distance from the edge of the substrate. In a second electroplating step, a second metal (e.g., tin) is electrodeposited using a lipseal that has an innermost point of contact with the semiconductor substrate at a greater distance from the edge of the substrate than the first distance. This allows to at least partially shift the lipseal pressure from a point that could have been damaged during the first electrodeposition step and to shield from electrolyte any cracks that might have formed in the mask material during the first electroplating step.