The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 01, 2017

Filed:

Mar. 20, 2014
Applicants:

Nippon Steel & Sumikin Materials Co., Ltd., Tokyo, JP;

Nippon Steel & Sumitomo Metal Corporation, Chiyoda-Ku, Tokyo, JP;

Inventors:

Eiki Tsushima, Hokkaido, JP;

Shinkichi Murakami, Tokyo, JP;

Jun Nakatsuka, Tokyo, JP;

Kenichi Uemura, Tokyo, JP;

Takashi Iijima, Tokyo, JP;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C01B 31/00 (2006.01); H01M 8/02 (2016.01); C01B 31/04 (2006.01); H01M 8/0213 (2016.01); H01M 8/1018 (2016.01);
U.S. Cl.
CPC ...
C01B 31/00 (2013.01); C01B 31/04 (2013.01); H01M 8/0213 (2013.01); C01P 2006/40 (2013.01); H01M 2008/1095 (2013.01);
Abstract

A thin-plate-like flexible carbon plate having flexibility, excellent compressive strength, and even electrical conductivity is provided. A carbon plateis a carbon plate having a thickness of 0.05 to 2.0 mm obtained by compression molding of a mixture of (a) 97 to 80 wt % carbon powder composed of 95 to 30 wt % expanded graphite powder and 5 to 70 wt % graphite powder, and (b) 3 to 20 wt % phenolic resin that do not contain ammonia, wherein a compressive strength is 3 MPa or more, a bending strain is 0.6% or more without a crack, and a contact resistance is 6 mΩ·cmor less.


Find Patent Forward Citations

Loading…