The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Mar. 21, 2017
Filed:
Sep. 05, 2008
Kayo Nakano, Yokohama, JP;
Akira Sato, Yokohama, JP;
Yasuhiro Shirakawa, Yokohama, JP;
Keiichi Fuse, Yokohama, JP;
Masami Okamura, Yokohama, JP;
Kayo Nakano, Yokohama, JP;
Akira Sato, Yokohama, JP;
Yasuhiro Shirakawa, Yokohama, JP;
Keiichi Fuse, Yokohama, JP;
Masami Okamura, Yokohama, JP;
KABUSHIKI KAISHA TOSHIBA, Tokyo, JP;
TOSHIBA MATERIALS CO., LTD., Yokohama-shi, JP;
Abstract
A visible-light-responsive photocatalyst powder includes a tungsten oxide powder. When the tungsten oxide powder is measured by X-ray diffractometry, (1) among intensity ratios of a peak A (2θ=22.8 to 23.4°), a peak B (2θ=23.4 to 23.8°), a peak C (2θ=24.0 to 24.25°), and a peak D (2θ=24.25 to 24.5°), an A/D ratio and a B/D ratio each fall within a range of 0.5 to 2.0, and a C/D ratio falls within a range of 0.04 to 2.5, (2) an intensity ratio (E/F) of a peak E (2θ=33.85 to 34.05°) to a peak F (2θ=34.05 to 34.25°) falls within a range of 0.1 to 2.0, and (3) an intensity ratio (G/H) of a peak G (2θ=49.1 to 49.7°) to a peak H (2θ=49.7 to 50.3°) falls within a range of 0.04 to 2.0, and the tungsten oxide powder has a BET specific surface area in a range of 1.5 to 820 m/g.