The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 07, 2017

Filed:

Mar. 30, 2010
Applicants:

Koji Hoshino, Kounosu, JP;

Ji-bin Yang, Okegawa, JP;

Kenji Orito, Niigata, JP;

Shinichi Ohmori, Okegawa, JP;

Inventors:

Koji Hoshino, Kounosu, JP;

Ji-bin Yang, Okegawa, JP;

Kenji Orito, Niigata, JP;

Shinichi Ohmori, Okegawa, JP;

Assignee:
Attorneys:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C22C 1/08 (2006.01); B22F 3/11 (2006.01); H01G 9/008 (2006.01); B22F 7/00 (2006.01); B22F 9/04 (2006.01); C22C 1/04 (2006.01); C22C 21/00 (2006.01); H01G 11/68 (2013.01); H01G 11/70 (2013.01); H01M 4/66 (2006.01); H01M 4/80 (2006.01);
U.S. Cl.
CPC ...
H01G 9/016 (2013.01); B22F 3/1125 (2013.01); B22F 7/006 (2013.01); B22F 9/04 (2013.01); C22C 1/0416 (2013.01); C22C 1/08 (2013.01); C22C 21/00 (2013.01); C22C 21/003 (2013.01); H01G 11/68 (2013.01); H01G 11/70 (2013.01); H01M 4/661 (2013.01); H01M 4/80 (2013.01); H01M 4/803 (2013.01); B22F 2998/00 (2013.01); Y02E 60/13 (2013.01); Y10T 428/12479 (2015.01);
Abstract

This method for producing porous sintered aluminum includes: mixing aluminum powder with a sintering aid powder containing a sintering aid element to obtain a raw aluminum mixed powder; forming the raw aluminum mixed powder into a formed object prior to sintering having pores; and heating the formed object prior to sintering in a non-oxidizing atmosphere to produce porous sintered aluminum, wherein the sintering aid element is titanium, and when a temperature at which the raw aluminum mixed powder starts to melt is expressed as Tm (° C.), then a temperature T (° C.) of the heating fulfills Tm-10 (° C.)≦T≦685 (° C.).