The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 13, 2016

Filed:

Apr. 21, 2015
Applicant:

Jgc Catalysts and Chemicals Ltd., Kawasaki-shi, JP;

Inventors:

Yoichi Ishihara, Kitakyushu, JP;

Hiroyasu Nishida, Kitakyushu, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08K 3/36 (2006.01); C09D 183/04 (2006.01); C01B 33/141 (2006.01); C09C 1/30 (2006.01); C09D 7/12 (2006.01); C09D 183/02 (2006.01); C09D 183/14 (2006.01); C01B 33/145 (2006.01); B82Y 30/00 (2011.01); C09D 133/00 (2006.01); C09D 163/00 (2006.01); C09D 167/00 (2006.01); C09D 175/04 (2006.01); C09D 179/04 (2006.01); C08G 77/58 (2006.01); C08K 9/02 (2006.01);
U.S. Cl.
CPC ...
C09D 183/04 (2013.01); B82Y 30/00 (2013.01); C01B 33/141 (2013.01); C01B 33/145 (2013.01); C09C 1/3054 (2013.01); C09D 7/1225 (2013.01); C09D 7/1266 (2013.01); C09D 133/00 (2013.01); C09D 163/00 (2013.01); C09D 167/00 (2013.01); C09D 175/04 (2013.01); C09D 179/04 (2013.01); C09D 183/02 (2013.01); C09D 183/14 (2013.01); C01P 2004/32 (2013.01); C01P 2004/64 (2013.01); C08G 77/58 (2013.01); C08K 3/36 (2013.01); C08K 9/02 (2013.01);
Abstract

Provided are silica-based fine particle dispersion sols, processes for producing the sols, coating compositions containing the dispersion sol, curable coating films obtained from the coating composition, and substrates having the coating film. The process including (1) mixing an aqueous aluminate solution to an alkaline silica sol which contains water-dispersible silica fine particles in a given ratio; (2) heating the mixture liquid obtained in step (1) to 60 to 200° C. and stirring the mixture liquid at the temperature for 0.5 to 20 hours; and (3) contacting the mixture liquid obtained in step (2) with a cation exchange resin to remove by ion exchange alkali metal ions contained in the mixture liquid and thereby controlling the pH of the mixture liquid to be in the range of 3.0 to 6.0.