The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 02, 2015

Filed:

Sep. 11, 2012
Applicants:

Takuro Homma, Tokyo, JP;

Katsuhiko Hotta, Tokyo, JP;

Takashi Moriyama, Tokyo, JP;

Inventors:

Takuro Homma, Tokyo, JP;

Katsuhiko Hotta, Tokyo, JP;

Takashi Moriyama, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01L 23/48 (2006.01); H01L 23/31 (2006.01); H01L 21/66 (2006.01); H01L 23/00 (2006.01);
U.S. Cl.
CPC ...
H01L 23/3192 (2013.01); H01L 22/32 (2013.01); H01L 24/03 (2013.01); H01L 24/06 (2013.01); H01L 24/45 (2013.01); H01L 2224/0401 (2013.01); H01L 2224/04042 (2013.01); H01L 2224/05552 (2013.01); H01L 2224/05567 (2013.01); H01L 2224/05571 (2013.01); H01L 2224/05624 (2013.01); H01L 2224/45144 (2013.01); H01L 2224/48091 (2013.01); H01L 2224/48227 (2013.01); H01L 2224/48228 (2013.01); H01L 2924/01004 (2013.01); H01L 2924/01005 (2013.01); H01L 2924/01007 (2013.01); H01L 2924/01013 (2013.01); H01L 2924/01014 (2013.01); H01L 2924/01015 (2013.01); H01L 2924/01018 (2013.01); H01L 2924/01022 (2013.01); H01L 2924/01025 (2013.01); H01L 2924/01027 (2013.01); H01L 2924/01029 (2013.01); H01L 2924/01033 (2013.01); H01L 2924/01047 (2013.01); H01L 2924/01051 (2013.01); H01L 2924/01074 (2013.01); H01L 2924/01079 (2013.01); H01L 2924/01082 (2013.01); H01L 2924/014 (2013.01); H01L 2924/04941 (2013.01); H01L 2924/05042 (2013.01); H01L 2924/10253 (2013.01); H01L 2924/13091 (2013.01); H01L 2924/14 (2013.01); H01L 2924/15311 (2013.01); H01L 2924/19041 (2013.01); H01L 2924/19043 (2013.01); H01L 24/48 (2013.01); H01L 2924/01006 (2013.01); H01L 2924/01019 (2013.01); H01L 2924/01045 (2013.01); H01L 2224/73265 (2013.01); H01L 2224/32225 (2013.01); H01L 2224/48624 (2013.01); H01L 2224/05553 (2013.01);
Abstract

In manufacturing an LSI, or semiconductor integrated circuit device, the step of assembling device (such as resin sealing step) is normally followed by a voltage-application test in an environment of high temperature (e.g., from 85 to 130° C.) and high humidity (e.g., about 80% RH). It has been found that separation of a titanium nitride anti-reflection film from an upper film and generation of cracks in the titanium nitride film at an upper surface edge part of the aluminum-based bonding pad applied with a positive voltage in the test is caused by an electrochemical reaction due to moisture incoming through the sealing resin and the like to generate oxidation and bulging of the titanium nitride film. These problems are addressed by removing the titanium nitride film over the pad in a ring or slit shape at peripheral area of the aluminum-based bonding pad.


Find Patent Forward Citations

Loading…