The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 30, 2014

Filed:

Jul. 23, 2010
Applicants:

Mark D. Alper, Mukwonago, WI (US);

Monina D. Kanderski, Milwaukee, WI (US);

Inventors:

Mark D. Alper, Mukwonago, WI (US);

Monina D. Kanderski, Milwaukee, WI (US);

Assignee:

Bostik, Inc., Wauwatosa, WI (US);

Attorneys:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B32B 7/12 (2006.01); B32B 5/26 (2006.01); B32B 27/12 (2006.01); B32B 27/32 (2006.01); C09J 153/00 (2006.01); C08L 53/02 (2006.01); D04H 1/42 (2012.01);
U.S. Cl.
CPC ...
D04H 1/42 (2013.01); B32B 2309/14 (2013.01); B32B 2255/02 (2013.01); B32B 27/12 (2013.01); B32B 2307/51 (2013.01); B32B 7/12 (2013.01); B32B 2255/10 (2013.01); B32B 2274/00 (2013.01); B32B 2255/26 (2013.01); C09J 153/00 (2013.01); C08L 53/02 (2013.01); B32B 2272/00 (2013.01); B32B 27/32 (2013.01); B32B 5/26 (2013.01); B32B 2555/02 (2013.01); B32B 2262/00 (2013.01);
Abstract

A hot melt adhesive composition, comprising a blend of components including about 5% to about 50% by weight of an olefin block copolymer; about 10% to about 70% by weight of a first tackifying resin having a softening point of at least about 95° C.; about 0 to 65% of a second tackifying resin that is different than the first tackifying resin; about 0% to about 60% by weight of a plasticizer; about 0% to about 20% by weight of an aromatic reinforcing resin having a softening point equal to or higher than 115° C.; about 0.1% to about 5% by weight of a stabilizer; and about 1% to about 40% by weight of a secondary polymer that is different from the olefin block copolymer, the first and second tackifying resins and the reinforcing resin, having relatively low crystallinity, which low crystallinity is equal to or less than 250 Joules/gram, wherein the components total 100% by weight of the composition, and the viscosity of the composition is equal to or less than about 20,000 mPa·s at 163° C. Laminates, especially those used in disposable soft goods, and methods of making such laminates using the hot melt adhesive composition are also described. The adhesive composition and/or laminate may be used in making a variety of end products such as a disposable diaper, a sanitary napkin, a bed pad, a bandage, a surgical drape, a tape, a label, a plastic sheet, a nonwoven sheet, a paper sheet, a cardboard, a book, a filter, or a package.