The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Jun. 04, 2002
Filed:
Apr. 06, 2001
In-sang Jeon, Suwon, KR;
Sang-bom Kang, Seoul, KR;
Hyun-seok Lim, Yongin, KR;
Gil-heyun Choi, Sungnam, KR;
Samsung Electronics Co., Ltd., Suwon, KR;
Abstract
A method of manufacturing a barrier metal layer uses atomic layer deposition (ALD) as the mechanism for depositing the barrier metal. The method includes supplying a first source gas onto the entire surface of a semiconductor substrate in the form of a pulse, and supplying a second source gas, which reacts with the first source gas, onto the entire surface of the semiconductor substrate in the form of a pulse. In a first embodiment, the pulses overlap in time so that the second source gas reacts with part of the first source gas physically adsorbed at the surface of the semiconductor substrate to thereby form part of the barrier metal layer by chemical vapor deposition whereas another part of the second source gas reacts with the first source gas chemically adsorbed at the surface of the semiconductor substrate to thereby form part of the barrier metal layer by atomic layer deposition. Thus, the deposition rate is greater than if the barrier metal layer were only formed by ALD. In the second embodiment, an impurity-removing gas is used to remove impurities in the barrier metal layer. Thus, even if the gas supply scheme is set up to only use ALD in creating the barrier metal layer, the deposition rate can be increased without the usual accompanying increase in the impurity content of the barrier metal layer.