The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 05, 1994

Filed:

Jul. 15, 1991
Applicant:
Inventors:

Norman A Card, Jr, Lockwood, NY (US);

Richard A Day, Whitney Point, NY (US);

Donald H Glatzel, New Milford, PA (US);

David J Russell, Apalachin, NY (US);

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
G03C / ;
U.S. Cl.
CPC ...
430280 ; 430311 ; 522 25 ; 522 49 ; 522 53 ; 522101 ;
Abstract

An improved photoimagable cationically polymerizable epoxy based coating material is provided. The material includes an epoxy resin system consisting essentially of between about 10% and about 80% by weight of a polyol resin which is a condensation product of epichlorohydrin and bisphenol A having a molecular weight of between about 40,000 and 130,000; between about 20% and about 90% by weight of an epoxidized octafunctional bisphenol A formaldehyde novolak resin having a molecular weight of 4,000 to 10,000; and if flame retardancy is required between about 35% and 50% by weight of an epoxidized glycidyl ether of tetrabromo bisphenol A having a softening point of between about 60 C. and about 110 C. and a molecular weight of between about 600 and 2,500. To this resin system is added about 0.1 to about 15 parts by weight per 100 parts of resin of a cationic photoinitiator capable of initiating polymerization of said epoxidized resin system upon exposure to actinic radiation; the system being further characterized by having an absorbance of light in the 330 to 700 nm region of less than 0.1 for a 2.0 mil thick film, and an effective amount of thixatropic agent. Optionally a photosensitizer such as perylene and its derivatives or anthracene and its derivatives may be added.


Find Patent Forward Citations

Loading…