The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 28, 2026

Filed:

Jan. 25, 2022
Applicants:

Tanaka Electronics Co., Ltd., Saga, JP;

Mitsubishi Electric Corporation, Tokyo, JP;

Inventors:

Shuichi Mitoma, Saga, JP;

Tsukasa Ichikawa, Saga, JP;

Tsuyoshi Uraji, Tokyo, JP;

Tatsunori Yanagimoto, Tokyo, JP;

Dai Nakajima, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22C 21/00 (2006.01); C22F 1/00 (2006.01); C22F 1/04 (2006.01); H10W 72/00 (2026.01); H10W 72/30 (2026.01); H10W 72/50 (2026.01); H10W 72/90 (2026.01); H10W 90/00 (2026.01);
U.S. Cl.
CPC ...
C22C 21/00 (2013.01); C22F 1/002 (2013.01); C22F 1/04 (2013.01); H10W 72/07533 (2026.01); H10W 72/07552 (2026.01); H10W 72/352 (2026.01); H10W 72/521 (2026.01); H10W 72/552 (2026.01); H10W 72/5524 (2026.01); H10W 72/884 (2026.01); H10W 72/90 (2026.01); H10W 72/923 (2026.01); H10W 72/944 (2026.01); H10W 72/952 (2026.01); H10W 90/734 (2026.01); H10W 90/736 (2026.01); H10W 90/753 (2026.01); H10W 90/754 (2026.01); H10W 90/756 (2026.01);
Abstract

An aluminum wire with which, at the time of bonding a bonding wire for a power semiconductor, the wire is not detached from a wedge tool, and a long life is achieved in a power cycle test. The aluminum wire is made of an aluminum alloy having an aluminum purity of 99 mass % or more and contains, relative to a total amount of all elements of the aluminum alloy, a total of 0.01 mass % or more and 1 mass % or less of iron and silicon. In a lateral cross-section in a direction perpendicular to a wire axis of the aluminum wire, an orientation index of is 1 or more, an orientation index of is 1 or less, and an area ratio of precipitated particles is in a range of 0.02% or more to 2% or less.