The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 16, 2026

Filed:

Nov. 24, 2021
Applicant:

Corning Incorporated, Corning, NY (US);

Inventors:

Ravindra Kumar Akarapu, San Diego, CA (US);

Matthew John Dejneka, Corning, NY (US);

Michael Edward Derosa, Painted Post, NY (US);

Diane Kimberlie Guilfoyle, Painted Post, NY (US);

Camden Wayne Isenberg, Sioux Falls, SD (US);

Manuela Ocampo Davila, Corning, NY (US);

Shawn Michael O'malley, Manchester, NH (US);

Paul George Rickerl, Endicott, NY (US);

Amber Leigh Tremper, Painted Post, NY (US);

Erick Franklin Vanduyne, Corning, NY (US);

Jonathan Earl Walter, Woodhull, NY (US);

Assignee:

CORNING INCORPORATED, Corning, NY (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 17/10 (2006.01); B32B 7/02 (2019.01); H05K 5/02 (2006.01); H05K 5/03 (2006.01);
U.S. Cl.
CPC ...
B32B 17/10045 (2013.01); B32B 7/02 (2013.01); B32B 17/101 (2013.01); B32B 17/10137 (2013.01); B32B 17/10651 (2013.01); B32B 17/10733 (2013.01); B32B 17/10743 (2013.01); B32B 17/10807 (2013.01); H05K 5/0217 (2013.01); H05K 5/03 (2013.01); B32B 2307/54 (2013.01); B32B 2307/558 (2013.01); B32B 2307/584 (2013.01); B32B 2307/7376 (2023.05); B32B 2457/20 (2013.01);
Abstract

Laminated glass-based articles are provided. The glass-based articles include at least a first glass-based layer, a second glass-based layer, and a polymer layer disposed between the first and second glass-based layers. The first glass-based layer includes a compressive stress. A difference between the coefficient of thermal of expansion of the first glass-based layer and the coefficient of thermal of expansion of the second glass-based layer is greater than or equal to 0.4 ppm/° C. Methods of producing the laminated glass-based articles are also provided.