The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 21, 2026

Filed:

Oct. 06, 2023
Applicant:

Samsung Electronics Co., Ltd., Suwon-si, KR;

Inventors:

Jinju Kim, Suwon-si, KR;

Kyunghwan Lee, Suwon-si, KR;

Cheolhee Cho, Suwon-si, KR;

Youngdeog Koh, Suwon-si, KR;

Kwangjoo Kim, Suwon-si, KR;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C25D 5/44 (2006.01); C23F 1/20 (2006.01); C25D 11/08 (2006.01); C25D 11/14 (2006.01); C25D 11/16 (2006.01); C25D 11/18 (2006.01); C25D 11/24 (2006.01);
U.S. Cl.
CPC ...
C25D 11/246 (2013.01); C23F 1/20 (2013.01); C25D 11/16 (2013.01); C25D 11/243 (2013.01);
Abstract

Disclosed is a method of treating a surface of an aluminum material, the method including: degreasing an aluminum material; etching the degreased aluminum material; performing a first desmutting treatment by immersing the etched aluminum material in a 25-35 wt % nitric acid solution at a temperature in a range of 25 to 30° C. for at least 60 seconds; performing a second desmutting treatment by immersing the first desmutting-treated aluminum material in a 5-15 wt % nitric acid solution at a temperature in a range of 25 to 30° C. for a time in a range of 30 seconds to 60 seconds; anodizing the second desmutting-treated aluminum material; coloring the anodized aluminum material; and sealing the colored aluminum material.


Find Patent Forward Citations