The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 21, 2026

Filed:

Apr. 25, 2022
Applicant:

Stratasys, Inc., Minnetonka, MN (US);

Inventors:

Fei Lin, Shanghai, CN;

Yifang Wang, Shanghai, CN;

Jie Qiao, Shanghai, CN;

Chenxi Zhang, Shanghai, CN;

Assignee:

Stratasys, Inc., Minnetonka, MN (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B29C 64/30 (2017.01); B29C 64/153 (2017.01); B29C 64/268 (2017.01); B29K 75/00 (2006.01); B33Y 10/00 (2015.01); B33Y 40/20 (2020.01); B33Y 70/00 (2020.01);
U.S. Cl.
CPC ...
B29C 64/30 (2017.08); B29C 64/153 (2017.08); B29C 64/268 (2017.08); B29K 2075/00 (2013.01); B33Y 10/00 (2014.12); B33Y 40/20 (2020.01); B33Y 70/00 (2014.12);
Abstract

The present invention relates to a method for producing an at least partially coated object and to an at least partially coated object obtained by the method. The method comprises bringing the object completely or partly into contact with a treating agent; leaving the object at 10° C.-30° C. and 100 mbar-800 mbar for 3-10 minutes; and heat-treating the object at a temperature of 70° C.-90° C. after returning to normal pressure; wherein the object is produced from a construction material by means of an additive manufacturing method, and the construction material comprises a thermoplastic polyurethane; and wherein the treating agent comprises an aqueous polyurethane dispersion and a water-dispersible polyisocyanate, and the viscosity of the treating agent is 100 mPa·s-550 mPa·s, measured under the condition of spindle L 2/30 rpm according to standard DIN 53019; and wherein the amount of the solid constituent of the aqueous polyurethane dispersion is 36% by weight to 70% by weight, and the amount of the solid constituent of the water-dispersible polyisocyanate is 4% by weight to 8% by weight, relative to the total weight of the treating agent, wherein the terms 'normal pressure' and “solid constituent” are defined as specified in the description. The at least partially coated object of the present invention has good mechanical properties and good surface effect.