The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 03, 2026

Filed:

Feb. 02, 2023
Applicant:

Shanghai Jiao Tong University, Shanghai, CN;

Inventors:

Haiyan Gao, Shanghai, CN;

Haiyang Lv, Shanghai, CN;

Mengmeng Wang, Shanghai, CN;

Peng Peng, Shanghai, CN;

Yun Wu, Shanghai, CN;

Chi Zhang, Shanghai, CN;

Min Li, Shanghai, CN;

Yufei Wang, Shanghai, CN;

Jun Wang, Shanghai, CN;

Baode Sun, Shanghai, CN;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C22C 21/00 (2006.01); B22F 1/05 (2022.01); B22F 1/065 (2022.01); B22F 9/08 (2006.01); B22F 10/28 (2021.01); B33Y 70/00 (2020.01); C22C 1/02 (2006.01); C22C 1/04 (2023.01); C22C 21/06 (2006.01);
U.S. Cl.
CPC ...
C22C 21/00 (2013.01); B22F 1/05 (2022.01); B22F 1/065 (2022.01); B22F 9/082 (2013.01); B33Y 70/00 (2014.12); C22C 1/026 (2013.01); C22C 1/0416 (2013.01); C22C 21/06 (2013.01); B22F 2009/0824 (2013.01); B22F 10/28 (2021.01); B22F 2301/052 (2013.01); B22F 2304/10 (2013.01);
Abstract

A method for preparing a rare earth aluminum alloy powder applicable for additive manufacturing includes: heating and melting aluminum ingots into an aluminum melt; adding required alloy elements to the aluminum melt to obtain an alloy melt in which the alloy elements are present in the following preset percentages by weight: 1.00% to 10.00% of Ce, 0.05% to 8.00% of Mg, 0.10% to 7.50% of Y, 0.10% to 2.50% of Zr, less than 0.1% of impurities, and the balance aluminum; leading out the alloy melt through a fluid guiding pipe, and impacting the alloy melt with a high-pressure gas flow so that the alloy melt is atomized into fine droplets under an action of surface tension, and solidified into spherical alloy powder; and collecting the spherical alloy powder in a vacuum collector, and screening and drying the spherical alloy powder to obtain the rare earth aluminum alloy powder.