The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 29, 2025

Filed:

Jan. 22, 2016
Applicant:

Bostik, Inc., Wauwatosa, WI (US);

Inventors:

Monina D. Kanderski, Milwaukee, WI (US);

Michael D. Vitrano, West Allis, WI (US);

Assignee:

Bostik, Inc., Wauwatosa, WI (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C09J 123/08 (2006.01); B32B 27/08 (2006.01); B32B 27/32 (2006.01); C08K 5/00 (2006.01); C08L 91/06 (2006.01);
U.S. Cl.
CPC ...
C09J 123/0815 (2013.01); B32B 27/08 (2013.01); B32B 27/32 (2013.01); B32B 27/327 (2013.01); C08K 5/005 (2013.01); C08L 91/06 (2013.01); B32B 2250/242 (2013.01); B32B 2439/70 (2013.01); C08L 2203/162 (2013.01);
Abstract

A low activation temperature heat seal hot melt adhesive for packaging applications based on a blend of metallocene catalyzed polyolefin polymer, tackifying resin, wax and other optional additives. In order to achieve the high viscosity suitable for an extrusion heat seal application, the adhesive composition of the invention is highly loaded with polymer, and thus should have a viscosity of about 50,000 centipoise or more measured at a temperature of 300° F. Accordingly, the hot melt adhesive composition contains about 50% to about 90% by weight of metallocene catalyzed polyolefin polymer, about 5% to about 50% by weight of tackifying resin, about 0.5% to about 40% by weight of wax, about 0.1% to about 5% by weight of a stabilizer or antioxidant, and 0% to about 25% by weight of optional additives. The hot melt adhesive composition must have an activation temperature of about 160° F. or less, and provide a minimum peel force of about 1.0 pound per inch in order to meet the sealing performance requirements for packaging food and other consumer goods.