The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 15, 2025

Filed:

Dec. 12, 2022
Applicant:

Wuhan Research Institute of Materials Protection, Wuhan, CN;

Inventors:

Haitao Duan, Wuhan, CN;

Changxin Wan, Wuhan, CN;

Shengpeng Zhan, Wuhan, CN;

Dan Jia, Wuhan, CN;

Jian Li, Wuhan, CN;

Wulin Zhang, Wuhan, CN;

Tian Yang, Wuhan, CN;

Yinhua Li, Wuhan, CN;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C10M 111/04 (2006.01); B29C 43/00 (2006.01); C08G 73/10 (2006.01); C08K 3/04 (2006.01); C10M 103/02 (2006.01); C10M 107/44 (2006.01); C10M 177/00 (2006.01); B29K 79/00 (2006.01); B29K 105/16 (2006.01); B29K 507/04 (2006.01); C10N 50/08 (2006.01); C10N 70/00 (2006.01);
U.S. Cl.
CPC ...
C10M 111/04 (2013.01); B29C 43/003 (2013.01); C08G 73/1035 (2013.01); C08G 73/1042 (2013.01); C08G 73/1071 (2013.01); C08K 3/042 (2017.05); C08K 3/046 (2017.05); C10M 103/02 (2013.01); C10M 107/44 (2013.01); C10M 177/00 (2013.01); B29K 2079/08 (2013.01); B29K 2105/162 (2013.01); B29K 2507/04 (2013.01); C08K 2201/011 (2013.01); C10M 2201/0413 (2013.01); C10M 2217/0415 (2013.01); C10N 2050/08 (2013.01); C10N 2070/00 (2013.01);
Abstract

This invention provides a preparation method of solid self-lubricating material with high temperature resistance, including steps described as follows: first, mixing polymer matrix resin and nano lubricating filler to compose a uniform raw material powders; then, placing the raw material powders in the cavity of hot-press die; keeping the temperature for 90-120 min at the first prepressing temperature, controlling the hot-pressing pressure under the third pre-loading pressure, and gradually increasing the temperature to the solid-phase molding temperature of the material; gradually reducing the temperature to the first preloading temperature after the solid-phase molding is completed; next, removing the pressure, finally, obtaining the solid self-lubricating material by naturally cooling to normal temperature and demoulding. This invention adjusts the hot-pressing molding temperature according to the drift value of glass transition temperature, in order to avoid the degradation of tribological properties and mechanical properties caused by uneven plasticization and overheating of composite materials during the compression molding process.