The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 25, 2025

Filed:

May. 14, 2020
Applicant:

Panasonic Intellectual Property Management Co., Ltd., Osaka, JP;

Inventors:

Yuki Kitai, Osaka, JP;

Masashi Koda, Fukushima, JP;

Yasunori Hoshino, Osaka, JP;

Atsushi Wada, Osaka, JP;

Mikio Sato, Fukushima, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 15/08 (2006.01); C08J 7/06 (2006.01); H05K 1/03 (2006.01); H05K 1/09 (2006.01); H05K 3/02 (2006.01);
U.S. Cl.
CPC ...
B32B 15/08 (2013.01); C08J 7/06 (2013.01); H05K 1/0353 (2013.01); H05K 1/09 (2013.01); H05K 3/022 (2013.01); B32B 2457/08 (2013.01); C08J 2325/06 (2013.01); H05K 2201/0355 (2013.01); H05K 2201/0358 (2013.01); H05K 2203/0392 (2013.01); H05K 2203/125 (2013.01); H05K 2203/1377 (2013.01);
Abstract

A copper clad laminate includes: an insulating layer containing a cured product of a resin composition; and a surface treated copper foil on one surface or both surfaces of the insulating layer, the resin composition containing a polymer, and the surface treated copper foil including a finely roughened particle treatment layer of copper on at least one surface side of a copper foil, the finely roughened particle treatment layer being formed of fine copper particles having a particle size of 40 to 200 nm, a heat resistance treatment layer containing nickel provided on the finely roughened particle treatment layer, a rust prevention treatment layer containing at least chromium provided on the heat resistance treatment layer, a silane coupling agent layer provided on the rust prevention treatment layer, and an amount of nickel attached in the heat resistance treatment layer being 30 to 60 mg/m.