The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 07, 2022

Filed:

Sep. 12, 2017
Applicant:

Panasonic Intellectual Property Management Co., Ltd., Osaka, JP;

Inventors:

Yuki Kitai, Osaka, JP;

Hiroaki Fujiwara, Nara, JP;

Mikio Sato, Osaka, JP;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B32B 15/04 (2006.01); B32B 15/08 (2006.01); B32B 27/08 (2006.01); H05K 1/03 (2006.01); H05K 1/09 (2006.01); C08F 290/06 (2006.01); B32B 27/00 (2006.01);
U.S. Cl.
CPC ...
B32B 15/04 (2013.01); B32B 15/08 (2013.01); B32B 27/00 (2013.01); B32B 27/08 (2013.01); C08F 290/06 (2013.01); C08F 290/062 (2013.01); H05K 1/03 (2013.01); H05K 1/0306 (2013.01); H05K 1/0313 (2013.01); H05K 1/09 (2013.01);
Abstract

A metal-clad laminate includes an insulating layer including a cured product of a resin composition, and a metal foil disposed on at least one principal surface of the insulating layer. The resin composition includes a thermosetting curing agent and a polyphenylene ether copolymer. The polyphenylene ether copolymer has an intrinsic viscosity ranging from 0.03 dl/g to 0.14 dl/g, inclusive. The intrinsic viscosity is measured in methylene chloride at 25° C. And the polyphenylene ether copolymer has, at a molecular terminal, a group represented by one of formula (1) and formula (2) at an average number of more than or equal to 0.8 and less than 1.5 per one molecule. Further, the metal foil includes a barrier layer containing cobalt on a first surface of the metal foil. The first surface is in contact with the insulating layer, and has a ten-point average roughness (Rz) of less than or equal to 2.0 μm. In formula (1), Rrepresents a hydrogen atom or an alkyl group having 1 to 10 carbon atoms, and Rrepresents an alkylene group having 1 to 10 carbon atoms. In formula (2), Rrepresents a hydrogen atom or an alkyl group having 1 to 10 carbon atoms.


Find Patent Forward Citations