The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 01, 2022

Filed:

Sep. 25, 2019
Applicant:

China Tobacco Yunnan Industrial Co., Ltd, Kunming, CN;

Inventors:

Ping Lei, Kunming, CN;

Jianguo Tang, Kunming, CN;

Yongkuan Chen, Kunming, CN;

Shanzhai Shang, Kunming, CN;

Xudong Zheng, Kunming, CN;

Zhiqiang Li, Kunming, CN;

Weimin Gong, Kunming, CN;

Jingmei Han, Kunming, CN;

Chengya Wang, Kunming, CN;

Jun Wu, Kunming, CN;

Pei He, Kunming, CN;

Xiaoli Xu, Kunming, CN;

Dongye Cao, Kunming, CN;

Zhihua Liu, Kunming, CN;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
A24B 15/16 (2020.01); A24D 1/22 (2020.01); C10L 5/44 (2006.01); C10L 9/10 (2006.01); C10L 10/00 (2006.01);
U.S. Cl.
CPC ...
A24B 15/165 (2013.01); A24D 1/22 (2020.01); C10L 5/44 (2013.01); C10L 9/10 (2013.01); C10L 10/00 (2013.01); C10L 2200/0254 (2013.01); C10L 2200/0469 (2013.01); C10L 2230/22 (2013.01); C10L 2270/08 (2013.01);
Abstract

A modified carbon material, including a carbonaceous material and a water-insoluble modifier combined with the carbonaceous material, wherein the water-insoluble modifier is CuO, the carbonaceous material is one of or a mixture of biomass carbon or carbon black, a mass of the water-insoluble modifier is being 0.1-10 wt % of the carbonaceous material. The method for preparing the modified carbon material includes: (1) soaking the carbonaceous material in a copper sulfate solution for 5 to 36 hours, and (2) adding an alkali solution into a solution obtained in step (1) to provide a pH value ≥12, and after keeping the pH value for 0.5 to 2 hours, filtering and drying to obtain a solid. (3) using the carbonaceous material as a combustion heat source to reduce the ignition temperature, increase or reduce the peak thermal power temperature.