The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 08, 2020

Filed:

Mar. 15, 2017
Applicant:

Meidensha Corporation, Tokyo, JP;

Inventors:

Shota Hayashi, Tokyo, JP;

Keita Ishikawa, Tokyo, JP;

Kenta Yamamura, Numazu, JP;

Kosuke Hasegawa, Numazu, JP;

Hideaki Fukuda, Numazu, JP;

Akira Sano, Fuji, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B22F 3/10 (2006.01); B22F 1/00 (2006.01); B22F 3/24 (2006.01); C22C 27/06 (2006.01); H01H 1/02 (2006.01); H01H 1/025 (2006.01); B22F 5/00 (2006.01); C22C 9/00 (2006.01); C22C 1/04 (2006.01); C22C 30/02 (2006.01); B22F 9/08 (2006.01); H01H 33/66 (2006.01); H01H 33/664 (2006.01); H01H 33/662 (2006.01);
U.S. Cl.
CPC ...
B22F 3/10 (2013.01); B22F 1/00 (2013.01); B22F 1/0003 (2013.01); B22F 3/24 (2013.01); B22F 5/00 (2013.01); B22F 9/08 (2013.01); C22C 1/04 (2013.01); C22C 9/00 (2013.01); C22C 27/06 (2013.01); C22C 30/02 (2013.01); H01H 1/025 (2013.01); H01H 1/0206 (2013.01); H01H 33/66 (2013.01); H01H 33/662 (2013.01); H01H 33/664 (2013.01);
Abstract

There is disclosed a method for manufacturing an electrode by pressing and sintering a mixed powder of a solid solution powder of Cr and a heat-resistant element, which contains Cr and the heat-resistant element in a ratio such that Cr is greater than the heat-resistant element by weight, a Cu powder, and a low melting metal powder (Bi, Sn, Se, Pb, etc.). The low melting metal powder of 0.30 weight % to 0.50 weight % is added to a mixed powder of a solid solution powder of Cr and the heat-resistant element and the Cu powder, and then a mixed powder prepared by adding the low melting metal powder is sintered at a temperature of from 1010° C. to 1035° C. As the low melting metal powder, there is used a powder having a median size of from 5 μm to 20 μm.


Find Patent Forward Citations

Loading…