The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 13, 2019

Filed:

Oct. 19, 2016
Applicant:

Denka Company Limited, Chuo-ku, Tokyo, JP;

Inventors:

Koki Ikarashi, Omuta, JP;

Shuhei Nonaka, Omuta, JP;

Toshikatsu Mitsunaga, Omuta, JP;

Hideki Hirotsuru, Omuta, JP;

Mitsuru Shiiba, Omuta, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C04B 35/583 (2006.01); C04B 41/00 (2006.01); C04B 41/84 (2006.01); C04B 41/83 (2006.01); C04B 41/48 (2006.01); C04B 41/49 (2006.01); H01L 23/14 (2006.01); H01L 23/373 (2006.01); H05K 1/03 (2006.01); C04B 111/00 (2006.01);
U.S. Cl.
CPC ...
C04B 41/84 (2013.01); C04B 35/583 (2013.01); C04B 41/009 (2013.01); C04B 41/48 (2013.01); C04B 41/4853 (2013.01); C04B 41/4905 (2013.01); C04B 41/4961 (2013.01); C04B 41/83 (2013.01); H01L 23/145 (2013.01); H01L 23/3737 (2013.01); H05K 1/0373 (2013.01); C04B 2111/00844 (2013.01); C04B 2235/3208 (2013.01); C04B 2235/386 (2013.01); C04B 2235/3895 (2013.01); C04B 2235/5292 (2013.01); C04B 2235/5436 (2013.01); C04B 2235/5472 (2013.01); C04B 2235/787 (2013.01); C04B 2235/9607 (2013.01); H01L 2924/0002 (2013.01); H05K 2201/0209 (2013.01);
Abstract

A resin-impregnated boron nitride sintered body having superior thermal conductivity and superior strength, and a resin-impregnated boron nitride sintered body having superior conductivity and small anisotropy of thermal conductivity are provided. A resin-impregnated boron nitride sintered body, including: 30 to 90 volume % of a boron nitride sintered body having boron nitride particles bonded three-dimensionally; and 10 to 70 volume % of a resin; wherein the boron nitride sintered body has a porosity of 10 to 70%; the boron nitride particles of the boron nitride sintered body has an average long diameter of 10 μm or more; the boron nitride sintered body has a graphitization index by powder X-ray diffractometry is 4.0 or less; and an orientation degree of the boron nitride particles of the boron nitride sintered body by I.O.P is 0.01 to 0.05 or 20 to 100; and a resin-impregnated boron nitride sintered body, including: 30 to 90 volume % of a boron nitride sintered body having boron nitride particles bonded three-dimensionally is provided.