The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 08, 2019

Filed:

Feb. 26, 2016
Applicant:

Nippon Yttrium Co., Ltd., Omuta-shi, Fukuoka, JP;

Inventors:

Naoki Fukagawa, Omuta, JP;

Yuji Shigeyoshi, Omuta, JP;

Assignee:

NIPPON YTTRIUM CO., LTD., Omuta-Shi, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C04B 35/553 (2006.01); C04B 35/505 (2006.01); C04B 35/50 (2006.01); C04B 35/622 (2006.01); C04B 35/626 (2006.01); C04B 35/634 (2006.01); C04B 35/64 (2006.01); B01J 2/00 (2006.01); C01F 17/00 (2006.01);
U.S. Cl.
CPC ...
C04B 35/553 (2013.01); B01J 2/00 (2013.01); C01F 17/0062 (2013.01); C04B 35/50 (2013.01); C04B 35/622 (2013.01); C04B 35/6262 (2013.01); C04B 35/62655 (2013.01); C04B 35/62675 (2013.01); C04B 35/62695 (2013.01); C04B 35/6342 (2013.01); C04B 35/63416 (2013.01); C04B 35/63424 (2013.01); C04B 35/63444 (2013.01); C04B 35/63488 (2013.01); C04B 35/64 (2013.01); C01P 2002/72 (2013.01); C01P 2002/74 (2013.01); C01P 2004/61 (2013.01); C01P 2004/62 (2013.01); C01P 2006/11 (2013.01); C04B 2235/3224 (2013.01); C04B 2235/3225 (2013.01); C04B 2235/3229 (2013.01); C04B 2235/445 (2013.01); C04B 2235/48 (2013.01); C04B 2235/5436 (2013.01); C04B 2235/5445 (2013.01); C04B 2235/604 (2013.01); C04B 2235/656 (2013.01); C04B 2235/721 (2013.01); C04B 2235/77 (2013.01); C04B 2235/80 (2013.01);
Abstract

The present invention is a sintering material including a granule, the sintering material having an apparent tap density of 1.0 to 2.5 g/cm, a 50% cumulative volume particle diameter (D) of 10 to 100 μm as measured before ultrasonication by laser diffraction/scattering particle size distribution analysis, a 50% cumulative volume particle diameter (D) of 0.1 to 1.5 μm as measured after ultrasonication at 300 W for 15 minutes by laser diffraction/scattering particle size distribution analysis, and an X-ray diffraction pattern in which the maximum peak observed in the 2θ angle range of from 20° to 40° is assigned to a rare earth oxyfluoride of the form LnOF when analyzed by X-ray diffractometry using Cu—Kα or Cu—Kαrays.