The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 17, 2018

Filed:

Apr. 11, 2016
Applicant:

3m Innovative Properties Company, Saint Paul, MN (US);

Inventors:

Jinbo Li, Shanghai, CN;

Jie Zhou, Shanghai, CN;

Rui Pan, Shanghai, CN;

Jiayun Zhu, Shanghai, CN;

Qisheng Pan, Shanghai, CN;

Xianfeng Ji, Beijing, CN;

Susannah C. Clear, Hastings, MN (US);

Gregory A. Shipp, Madison, CT (US);

Yingyu Wang, Shanghai, CN;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01L 31/048 (2014.01); C09J 7/02 (2006.01);
U.S. Cl.
CPC ...
H01L 31/0481 (2013.01); C09J 7/025 (2013.01); C09J 7/0257 (2013.01); C09J 7/0278 (2013.01); C09J 7/0292 (2013.01); C09J 2201/134 (2013.01); C09J 2203/322 (2013.01); C09J 2400/163 (2013.01); C09J 2423/045 (2013.01); C09J 2423/105 (2013.01); C09J 2427/006 (2013.01); C09J 2433/00 (2013.01); C09J 2467/001 (2013.01); Y10T 428/24802 (2015.01); Y10T 428/24843 (2015.01); Y10T 428/31678 (2015.04); Y10T 428/31826 (2015.04); Y10T 428/31855 (2015.04);
Abstract

The invention provides a frameless photo-energy assembly including a photo-energy converter, wherein an edge of the photo-energy converter is sealed by an adhesive tape, comprising an adhering layer for adhesion and cushioning; and an aging-resistant protective layer. The adhering layer is used to contact the edge of an article and comprises: a substrate layer; optionally, a first adhesive layer and a second adhesive layer situated at both sides of the substrate layer oppositely, wherein the first adhesive layer being used to be contact with the article. The aging-resistant protective layer is situated on the adhering layer, which comprises: an optional primer layer, which is situated on the adhering layer; and a film layer, which is situated on either the primer layer or the substrate or the second adhesive layer. The invention further provides an adhesive tape for sealing an edge of an article and an article made of the assembly.