The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 05, 2018

Filed:

Dec. 11, 2014
Applicants:

The Abbott Ball Company, West Hartford, CT (US);

Puris, Llc, Bruceton Mills, WV (US);

Inventors:

Glenn Glennon, West Hartford, CT (US);

Eric Bono, McDonald, PA (US);

Assignees:

THE ABBOTT BALL COMPANY, West Hartford, CT (US);

CARPENTER TECHNOLOGY CORPORATION, Philadelphia, PA (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22C 19/03 (2006.01); B32B 15/04 (2006.01); B32B 37/10 (2006.01); B32B 37/06 (2006.01); B32B 15/01 (2006.01); B05D 7/24 (2006.01); B05D 3/02 (2006.01); B05D 7/14 (2006.01); B23K 20/02 (2006.01); C23C 28/02 (2006.01); C23C 26/00 (2006.01); C23C 30/00 (2006.01); C22C 19/00 (2006.01); C23C 24/08 (2006.01);
U.S. Cl.
CPC ...
C22C 19/03 (2013.01); B23K 20/023 (2013.01); B32B 15/01 (2013.01); C22C 19/00 (2013.01); C22C 19/007 (2013.01); C23C 24/087 (2013.01); C23C 26/00 (2013.01); C23C 28/02 (2013.01); C23C 28/021 (2013.01); C23C 30/00 (2013.01); C23C 30/005 (2013.01); Y10T 428/12451 (2015.01); Y10T 428/12472 (2015.01); Y10T 428/12806 (2015.01); Y10T 428/12944 (2015.01); Y10T 428/12993 (2015.01);
Abstract

Disclosed herein is a method comprising disposing on a base article a nickel-titanium alloy; where the nickel is in an amount of about 58 to about 62 weight percent and titanium in an amount of about 38 to about 42 wt %, based on the total weight of the nickel-titanium alloy; and applying a pressure of 12 to 20 kilopounds per square inch at a temperature of 1400 to 2100° F. for a period of 1 to 8 hours to form a nickel-titanium alloy coating on the base article. Disclosed is an article comprising a base article; and a nickel-titanium alloy; where the nickel-titanium alloy is disposed on the base article; where the nickel is in an amount of about 58 to about 62 weight percent and titanium in an amount of about 38 to about 42 wt %, based on the total weight of the nickel-titanium alloy.