The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
May. 01, 2018
Filed:
May. 31, 2017
Applicant:
Arcelormittal, Luxembourg, LU;
Inventors:
Juan David Puerta Velasquez, Metz, FR;
Jonas Staudte, Montigny-les-Metz, FR;
Pascal Drillet, Rozerieulles, FR;
Assignee:
ArcelorMittal, Luxembourg, LU;
Primary Examiner:
Int. Cl.
CPC ...
C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/32 (2006.01); C21D 8/02 (2006.01); B32B 15/01 (2006.01); C23C 2/28 (2006.01); C22C 38/28 (2006.01); C22C 38/06 (2006.01); C22C 38/00 (2006.01); C21D 6/00 (2006.01); C23C 2/12 (2006.01); C23C 2/06 (2006.01);
U.S. Cl.
CPC ...
C21D 8/0278 (2013.01); B32B 15/012 (2013.01); B32B 15/013 (2013.01); C21D 6/002 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/0205 (2013.01); C21D 8/0236 (2013.01); C21D 8/0257 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/28 (2013.01); C22C 38/32 (2013.01); C23C 2/06 (2013.01); C23C 2/12 (2013.01); C23C 2/28 (2013.01);
Abstract
A cold-rolled sheet is provided. The cold-rolled sheet includes a steel substrate with a carbon content Cbetween 0.07% and 0.5%, expressed by weight, and a metal pre-coating on at least the two principal faces of the steel substrate. The substrate has a decarburized area on the surface of each of the two principal faces. The depth pof the decarburized area is between 6 and 30 micrometers, and pis the depth at which the carbon content is equal to 50% of the content C. The sheet does not contain a layer of iron oxide between the substrate and the metal pre-coating.