The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 01, 2018

Filed:

Dec. 13, 2013
Applicant:

Nippon Steel & Sumitomo Metal Corporation, Tokyo, JP;

Inventors:

Shigefumi Nishitani, Tokyo, JP;

Motoki Takasuga, Tokyo, JP;

Hitoshi Matsumoto, Tokyo, JP;

Tatsuya Hasegawa, Tokyo, JP;

Masato Yuya, Tokyo, JP;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C22C 38/00 (2006.01); B60W 10/26 (2006.01); B60W 10/24 (2006.01); B60W 20/00 (2016.01); C21D 9/00 (2006.01); C21D 9/30 (2006.01); C22C 38/60 (2006.01); C21D 1/06 (2006.01); C22C 38/02 (2006.01); C22C 38/20 (2006.01); C22C 38/22 (2006.01); C22C 38/28 (2006.01); C22C 38/38 (2006.01); C22C 38/42 (2006.01); C22C 38/58 (2006.01);
U.S. Cl.
CPC ...
B60W 10/26 (2013.01); B60W 10/24 (2013.01); B60W 20/00 (2013.01); C21D 1/06 (2013.01); C21D 9/00 (2013.01); C21D 9/30 (2013.01); C22C 38/00 (2013.01); C22C 38/001 (2013.01); C22C 38/02 (2013.01); C22C 38/20 (2013.01); C22C 38/22 (2013.01); C22C 38/28 (2013.01); C22C 38/38 (2013.01); C22C 38/42 (2013.01); C22C 38/58 (2013.01); C22C 38/60 (2013.01);
Abstract

Provided is a non-thermal refined soft-nitrided component including chemical composition of a steel material of a base metal containing: in mass %, C: 0.25 to 0.40%; Si: 0.10 to 0.35%; Mn: more than 2.0% to 2.8% or less; N: 0.0030 to 0.0250%; Cu: 0 to 1.0%; Mo: 0 to 0.3%; Ni: 0 to 0.5%; Ti: 0 to 0.020%; and a balance being Fe and impurities, the impurities including P: 0.08% or less; S: 0.10% or less; Al: 0.05% or less; and Cr: less than 0.20%, wherein a Vickers hardness at a position of 0.05 mm from the surface is 400 to 480, a Vickers hardness at a position of 1.0 mm from the surface is 200 or more, and a compound-layer depth at a stress concentrated region is 5 μm or less. This non-thermal refined soft-nitrided component has an excellent bending straightening property and a high fatigue strength.


Find Patent Forward Citations