The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 17, 2018

Filed:

Oct. 17, 2014
Applicant:

Lg Chem, Ltd., Seoul, KR;

Inventors:

Jinsoo Lee, Daejeon, KR;

Taesu Kim, Daejeon, KR;

Hyeran Jung, Daejeon, KR;

Bugon Shin, Daejeon, KR;

Assignee:

LG CHEM, LTD., Seoul, KR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 2/26 (2006.01); B23K 26/22 (2006.01); B23K 26/0622 (2014.01); B23K 26/323 (2014.01); H01M 10/04 (2006.01); H01M 4/75 (2006.01); B23K 26/20 (2014.01); B23K 26/40 (2014.01); H01M 4/70 (2006.01); B23K 26/00 (2014.01); B23K 26/354 (2014.01); B23K 26/60 (2014.01); H01M 2/22 (2006.01); H01M 4/66 (2006.01); H01M 4/74 (2006.01); B23K 101/38 (2006.01); B23K 103/16 (2006.01); B23K 103/08 (2006.01); B23K 103/00 (2006.01);
U.S. Cl.
CPC ...
H01M 2/26 (2013.01); B23K 26/0081 (2013.01); B23K 26/0622 (2015.10); B23K 26/20 (2013.01); B23K 26/22 (2013.01); B23K 26/323 (2015.10); B23K 26/354 (2015.10); B23K 26/40 (2013.01); B23K 26/60 (2015.10); H01M 2/22 (2013.01); H01M 4/661 (2013.01); H01M 4/667 (2013.01); H01M 4/70 (2013.01); H01M 4/75 (2013.01); H01M 10/0422 (2013.01); H01M 10/0436 (2013.01); B23K 2201/38 (2013.01); B23K 2203/08 (2013.01); B23K 2203/172 (2015.10); B23K 2203/50 (2015.10); H01M 4/74 (2013.01); H01M 2220/30 (2013.01);
Abstract

Disclosed are a method of welding a metal tab of an electrode layer for a cable battery and an electrode manufactured thereby. This welding method, suitable for welding a metal tab to an electrode including a current collector for a cable battery, a conductive layer formed on the outer surface of the current collector, and a polymer film layer formed on the inner surface of the current collector, includes: a) removing a portion of the conductive layer using a pulse laser, thus exposing the surface of the current collector positioned thereunder, and b) welding a metal tab to the surface of the current collector, thus enabling the welding of a metal tab and an electrode for a cable battery, which has been difficult to achieve using a conventional welding process.