The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 17, 2018

Filed:

Nov. 23, 2015
Applicant:

Celanese International Corporation, Irving, TX (US);

Inventors:

Matthias Junk, Alsbach-Hähnlein, DE;

Ulrich Desor, Idstein, DE;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08L 33/12 (2006.01); C08F 220/18 (2006.01); C08F 265/06 (2006.01); C08J 3/12 (2006.01); C09D 133/12 (2006.01); C08F 2/00 (2006.01); C09D 151/00 (2006.01); C09D 5/02 (2006.01);
U.S. Cl.
CPC ...
C08L 33/12 (2013.01); C08F 2/001 (2013.01); C08F 220/18 (2013.01); C08F 265/06 (2013.01); C08J 3/12 (2013.01); C09D 5/02 (2013.01); C09D 133/12 (2013.01); C09D 151/003 (2013.01); C08J 2333/12 (2013.01); C08L 2201/54 (2013.01); C08L 2205/025 (2013.01); C08L 2308/00 (2013.01);
Abstract

A polymer dispersion is produced by polymerization of at least two different ethylenically unsaturated monomers in at least first and second stages. The polymer produced in the first stage comprises 25 to 60% by weight of the total monomer composition and has a uniform glass transition temperature from −30° C. to 0° C. The polymer produced in the second stage comprises 40 to 75% by weight of the total monomer composition and has a variable monomer composition such that the second stage polymer has a non-uniform glass transition temperature which varies between a first value from −30° to +10° C. and second value of at least +70° C. Any polymer produced in further polymerization stages comprises no more than 10% by weight of the total monomer composition and the glass transition temperature of the hypothetical uniform copolymer produced by the total monomer composition is in the range from 0° C. to 25° C.