The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 13, 2018

Filed:

Sep. 28, 2012
Applicant:

Areva NP, Courbevoie, FR;

Inventor:

Dominique Hertz, Sainte Foy Les Lyon, FR;

Assignee:

AREVA NP, Courbevoie, FR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
G21C 3/06 (2006.01); G21C 7/10 (2006.01); C21D 1/72 (2006.01); C21D 6/00 (2006.01); C21D 9/08 (2006.01); C21D 9/14 (2006.01); C23C 8/02 (2006.01); C23C 8/32 (2006.01); C23C 8/80 (2006.01); G21C 21/18 (2006.01); C23C 8/22 (2006.01); C23C 8/38 (2006.01); G21C 7/06 (2006.01); C21D 8/10 (2006.01);
U.S. Cl.
CPC ...
C21D 1/72 (2013.01); C21D 6/004 (2013.01); C21D 9/08 (2013.01); C21D 9/085 (2013.01); C21D 9/14 (2013.01); C23C 8/02 (2013.01); C23C 8/22 (2013.01); C23C 8/32 (2013.01); C23C 8/38 (2013.01); C23C 8/80 (2013.01); G21C 7/06 (2013.01); G21C 7/10 (2013.01); G21C 21/18 (2013.01); C21D 8/10 (2013.01); C21D 8/105 (2013.01); Y02E 30/39 (2013.01);
Abstract

A method for producing a wear-resistant and corrosion-resistant stainless steel part for a nuclear reactor is provided. This method includes steps of providing a tubular blank in austenitic stainless steel whose carbon content is equal to or lower than 0.03% by weight; shaping the blank; finishing the blank to form the cladding; hardening the outer surface of the cladding by diffusing one or more atomic species; the blank, before the providing step or during the shaping or finishing step, being subjected to at least one hyper quenching with sub-steps of: heating the blank to a sufficient temperature and for a sufficient time to solubilize any precipitates present; quenching the blank at a rate allowing the austenitic structure to be maintained in a metastable state at ambient temperature and free of precipitates.