The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 06, 2018

Filed:

Aug. 27, 2014
Applicant:

Federal-mogul Corporation, Southfield, MI (US);

Inventors:

Zachary Odel Roelofs, Granger, IN (US);

Airton Martins, Granger, IN (US);

Ross Evers, Tecumseh, MI (US);

Oscar Garza, Puebla, MX;

Assignee:

Federal-Mogul LLC, Southfield, MI (US);

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
F02F 3/00 (2006.01); B23K 13/01 (2006.01); B23K 20/12 (2006.01); B23K 20/24 (2006.01); B23K 28/02 (2014.01); B21J 5/08 (2006.01); B21K 3/00 (2006.01); B23K 31/12 (2006.01); B23P 15/10 (2006.01); B23K 101/00 (2006.01);
U.S. Cl.
CPC ...
F02F 3/003 (2013.01); B21J 5/08 (2013.01); B21K 3/00 (2013.01); B23K 13/015 (2013.01); B23K 20/129 (2013.01); B23K 20/24 (2013.01); B23K 28/02 (2013.01); B23K 31/12 (2013.01); B23K 2201/003 (2013.01); B23P 15/10 (2013.01); F02F 2003/0061 (2013.01);
Abstract

A hybrid induction welded piston including an upper piston part welded to a lower piston part is provided. The piston is produced by induction heating the upper piston part and the lower piston part, and bringing the parts together to a part growth compensated position. The method then includes rotating the upper piston part 17 to 34 degrees clockwise and then 17 to 34 degrees counterclockwise. In addition to controlling the axial position and degree of rotation, the force applied to the piston parts is controlled so that preferably no flash is formed in a narrow cooling chamber of the piston. During the rotating steps, the pressure gradually increases to a maximum level which occurs while the upper piston part is rotating in the second direction. The piston includes a homogenous metallurgical bond across the weld and no indentation on the outer surface at the weld prior to machining.