The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 23, 2018

Filed:

Mar. 03, 2015
Applicant:

Nippon Shokubai Co., Ltd., Osaka-shi, Osaka, JP;

Inventors:

Satoshi Matsumoto, Himeji, JP;

Shinichi Fujino, Himeji, JP;

Kunihiko Ishizaki, Himeji, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B01J 20/26 (2006.01); A61L 15/24 (2006.01); A61L 15/60 (2006.01); C08F 220/06 (2006.01); C08J 3/075 (2006.01); B01J 20/30 (2006.01);
U.S. Cl.
CPC ...
B01J 20/267 (2013.01); A61L 15/24 (2013.01); A61L 15/60 (2013.01); B01J 20/3021 (2013.01); C08F 220/06 (2013.01); C08J 3/075 (2013.01); C08J 2333/02 (2013.01);
Abstract

To provide a method for producing a water-absorbing resin by which problems caused by addition of a particulate additive or water-absorbing resin fine powder can be prevented and a water-absorbing resin having high physical properties can be stably and efficiently obtained. A method for producing a polyacrylic acid (salt)-based water-absorbing resin, the method including: an aqueous monomer solution preparation step for preparing an aqueous solution containing a monomer having an acrylic acid (salt) as a main component; a polymerization step for polymerizing the monomer to obtain a hydrogel-forming crosslinked polymer; and a drying step for drying the hydrogel-forming crosslinked polymer to obtain a dry polymer, wherein the method further includes an adding step for adding a particulate additive to the aqueous monomer solution and/or the hydrogel-forming crosslinked polymer, and in the adding step, an oxygen concentration in an ambient atmosphere of the particulate additive is set to 5% by volume or less.