The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 09, 2018

Filed:

Jul. 30, 2012
Applicants:

Shinya Tabata, Kobe, JP;

Kazumasa Shintani, Kobe, JP;

Takuya Onimura, Kobe, JP;

Inventors:

Shinya Tabata, Kobe, JP;

Kazumasa Shintani, Kobe, JP;

Takuya Onimura, Kobe, JP;

Assignee:

SANTOKU CORPORATION, Kobe-shi, Hyogo, JP;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
H01F 1/20 (2006.01); B22D 11/00 (2006.01); C22C 38/10 (2006.01); C22C 38/16 (2006.01); H01F 1/057 (2006.01); B22D 11/06 (2006.01); C22C 38/00 (2006.01); C22C 38/06 (2006.01);
U.S. Cl.
CPC ...
H01F 1/20 (2013.01); B22D 11/0651 (2013.01); C22C 38/002 (2013.01); C22C 38/005 (2013.01); C22C 38/06 (2013.01); C22C 38/10 (2013.01); C22C 38/16 (2013.01); H01F 1/0571 (2013.01); H01F 1/0577 (2013.01); C22C 2202/02 (2013.01);
Abstract

Provided are raw material alloy flakes for a rare earth sintered magnet and a method for producing the same. The alloy flakes have a roll-cooled face, and (1) contain at least one R selected from rare earth metal elements including Y, B, and the balance M including iron, at a particular ratio; (2) as observed in a micrograph at a magnification of 100× of its roll-cooled face, have not less than 5 crystals each of which is a dendrite grown radially from a point of crystal nucleation, and crosses a line segment corresponding to 880 μm; and (3) as observed in a micrograph at a magnification of 200× of its section taken generally perpendicularly to its roll-cooled face, have an average distance between R-rich phases of not less than 1 μm and less than 10 μm.