The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 12, 2017

Filed:

Feb. 25, 2013
Applicant:

Jfe Steel Corporation, Chiyoda-ku, Tokyo, JP;

Inventors:

Daisuke Harako, Kawasaki, JP;

Yoshitsugu Suzuki, Fukuyama, JP;

Yasunobu Nagataki, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 15/00 (2006.01); C21D 8/00 (2006.01); C23C 2/02 (2006.01); C23C 2/06 (2006.01); C21D 9/46 (2006.01); C22C 38/14 (2006.01); C23C 28/00 (2006.01); C21D 8/02 (2006.01); B32B 15/01 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/12 (2006.01); C22C 38/06 (2006.01); C23F 17/00 (2006.01); C23C 2/28 (2006.01); C21D 9/56 (2006.01); C22C 18/00 (2006.01);
U.S. Cl.
CPC ...
C21D 8/005 (2013.01); B32B 15/01 (2013.01); B32B 15/013 (2013.01); C21D 8/0205 (2013.01); C21D 8/0263 (2013.01); C21D 8/0278 (2013.01); C21D 9/46 (2013.01); C21D 9/561 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/12 (2013.01); C22C 38/14 (2013.01); C23C 2/02 (2013.01); C23C 2/06 (2013.01); C23C 2/28 (2013.01); C23C 28/321 (2013.01); C23C 28/345 (2013.01); C23F 17/00 (2013.01); C21D 2241/00 (2013.01); C22C 18/00 (2013.01); Y10T 428/12799 (2015.01);
Abstract

A high strength galvanized steel sheet has a composition including, C: 0.02% or more and 0.30% or less, Si: 0.01% or more and 2.5% or less, Mn: 0.1% or more and 3.0% or less, P: 0.003% or more and 0.08% or less, S: 0.01% or less, Al: 0.001% or more and 0.20% or less, Ti: 0.03% or more and 0.40% or less and the balance being Fe and inevitable impurities, and a zinc-coated layer having a coating weight per surface of 20 g/mor more and 120 g/mor less. The concentration ratio of C to Ti (C/Ti) in a portion within 10 μm from the surface of the base steel sheet is 0.8 or more and 1.5 or less, and the total amount of oxides of one or more selected from Fe, Si, Mn, P, Al and Ti formed in a surface portion within 100 μm from the surface of the base steel sheet is 0.05 g/mor less.