The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 28, 2017

Filed:

Dec. 19, 2012
Applicant:

Sandvik Intellectual Property Ab, Sandviken, SE;

Inventors:

Andreas Hedin, Stockholm, SE;

Susanne Norgren, Huddinge, SE;

Nina Sjodahl, Stockholm, SE;

Jose Garcia, Stockholm, SE;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B22F 3/12 (2006.01); B22F 8/00 (2006.01); C22C 29/02 (2006.01); B22F 9/04 (2006.01); B23B 51/00 (2006.01); B23C 5/10 (2006.01); B22F 5/00 (2006.01);
U.S. Cl.
CPC ...
B22F 8/00 (2013.01); B22F 3/12 (2013.01); B22F 9/04 (2013.01); B23B 51/00 (2013.01); B23C 5/10 (2013.01); C22C 29/02 (2013.01); B22F 2005/001 (2013.01); B22F 2009/041 (2013.01); B22F 2009/043 (2013.01); B22F 2302/10 (2013.01); B22F 2302/15 (2013.01); B22F 2303/01 (2013.01); B22F 2303/05 (2013.01); B22F 2998/00 (2013.01); B22F 2998/10 (2013.01); B23B 2222/28 (2013.01); B23C 2222/28 (2013.01); Y02P 10/24 (2015.11); Y02W 30/541 (2015.05); Y10T 407/27 (2015.01);
Abstract

The present invention relates to a method of making a cemented carbide comprising mixing in a slurry a first powder fraction and a second powder fraction, subjecting the slurry to milling, drying, pressing and sintering. The first powder fraction is made from cemented carbide scrap recycled using the Zn recovery process, comprising the elements W, C, Co, and at least one or more of Ta, Ti, Nb, Cr, Zr, Hf and Mo, and the second powder fraction comprising virgin raw materials of WC and possibly carbides and/or carbonitrides of one or more of Cr, Zr, W, Ta, Ti, Hf and Nb. The first powder fraction is subjected to a pre-milling step, prior to the step of forming the slurry, to obtain an average grain size of between 0.2 to 1.5 μm.


Find Patent Forward Citations

Loading…