The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 07, 2017

Filed:

Jan. 21, 2010
Applicants:

Shyam S. Bayya, Ashburn, VA (US);

Woohong Kim, Lorton, VA (US);

Jasbinder S. Sanghera, Ashburn, VA (US);

Guillermo R. Villalobos, Springfield, VA (US);

Ishwar D. Aggarwal, Fairfax Station, VA (US);

Inventors:

Shyam S. Bayya, Ashburn, VA (US);

Woohong Kim, Lorton, VA (US);

Jasbinder S. Sanghera, Ashburn, VA (US);

Guillermo R. Villalobos, Springfield, VA (US);

Ishwar D. Aggarwal, Fairfax Station, VA (US);

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
C04B 35/51 (2006.01); C04B 35/547 (2006.01); B82Y 30/00 (2011.01); C01F 17/00 (2006.01); C04B 35/626 (2006.01); C04B 35/645 (2006.01);
U.S. Cl.
CPC ...
C04B 35/547 (2013.01); B82Y 30/00 (2013.01); C01F 17/0037 (2013.01); C04B 35/62665 (2013.01); C04B 35/645 (2013.01); C01P 2002/72 (2013.01); C01P 2004/03 (2013.01); C01P 2004/64 (2013.01); C01P 2006/12 (2013.01); C01P 2006/80 (2013.01); C04B 2235/3208 (2013.01); C04B 2235/3224 (2013.01); C04B 2235/3227 (2013.01); C04B 2235/443 (2013.01); C04B 2235/5409 (2013.01); C04B 2235/5454 (2013.01); C04B 2235/658 (2013.01); C04B 2235/72 (2013.01); C04B 2235/721 (2013.01); C04B 2235/9653 (2013.01); C04B 2235/9661 (2013.01);
Abstract

A method of preparing a fine powder of calcium lanthanoid sulfide is disclosed. The method includes spraying soluble calcium and lanthanoid salts into at least one precipitating solution to form a precipitate comprising insoluble calcium and lanthanoid salts, optionally, oxidizing the precipitate comprising insoluble calcium and lanthanoid salts, and sulfurizing the optionally oxidized precipitate to form a fine powder of calcium lanthanoid sulfide. An alternative method for forming the powder is by flame pyrolysis. The calcium lanthanoid sulfide powder produced by either method can have an impurity concentration of less than 100 ppm, a carbon concentration of less than 200 ppm, a BET surface area of at least 50 m/g, and an average particle size of less than 100 nm.