The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 24, 2017

Filed:

Mar. 12, 2014
Applicants:

Henk-jan Brinkman, Bonn, DE;

Dietmar Schröder, Grevenbroich, DE;

Thomas Wirtz, Hamburg, DE;

Natalie Hörster, Köln, DE;

Werner Kehl, Jork, DE;

Olaf Engler, Bonn, DE;

Inventors:

Henk-Jan Brinkman, Bonn, DE;

Dietmar Schröder, Grevenbroich, DE;

Thomas Wirtz, Hamburg, DE;

Natalie Hörster, Köln, DE;

Werner Kehl, Jork, DE;

Olaf Engler, Bonn, DE;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 15/01 (2006.01); B23K 20/233 (2006.01); C22C 1/05 (2006.01); C22C 21/00 (2006.01); C22C 21/08 (2006.01); C22F 1/04 (2006.01); C22F 1/05 (2006.01); B23K 20/04 (2006.01);
U.S. Cl.
CPC ...
B32B 15/016 (2013.01); B23K 20/04 (2013.01); B23K 20/2336 (2013.01); C22C 1/05 (2013.01); C22C 21/00 (2013.01); C22C 21/08 (2013.01); C22F 1/04 (2013.01); C22F 1/05 (2013.01); Y10T 428/12764 (2015.01);
Abstract

The invention relates to a strip consisting of an aluminum material for producing components with improved bending behavior and exacting shaping requirements, a method for producing the strip and the use of sheets produced from the strip according to the invention. The strip has a core layer of an AlMgSi alloy and at least one outer aluminum alloy layer arranged on one or both sides, made from a non-hardenable aluminum alloy, wherein the at least one outer aluminum layer has a lower tensile strength in the (T4) state than the AlMgSi layer, wherein the strip has a uniform strain (A) in the (T4) state of more than 23% transverse to the rolling direction and, at a thickness of 1.5 mm-1.6 mm, achieves a bending angle of less than 40° in a bending test.