The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 22, 2017

Filed:

Mar. 27, 2014
Applicant:

Kobe Steel, Ltd., Kobe-shi, JP;

Inventors:

Yoichi Takahashi, Takasago, JP;

Takuo Shigehisa, Takasago, JP;

Tsuyoshi Adachi, Kobe, JP;

Assignee:

Kobe Steel, Ltd., Kobe-shi, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C10L 5/02 (2006.01); C10L 5/06 (2006.01); B29C 67/00 (2017.01); C10L 5/08 (2006.01); C10L 5/04 (2006.01); C10L 9/00 (2006.01); C10L 5/36 (2006.01); C10L 9/10 (2006.01);
U.S. Cl.
CPC ...
C10L 5/08 (2013.01); C10L 5/04 (2013.01); C10L 5/361 (2013.01); C10L 9/00 (2013.01); C10L 9/10 (2013.01); C10L 2200/043 (2013.01); C10L 2290/06 (2013.01); C10L 2290/08 (2013.01); C10L 2290/18 (2013.01); C10L 2290/24 (2013.01); C10L 2290/28 (2013.01); C10L 2290/30 (2013.01); C10L 2290/32 (2013.01); C10L 2290/546 (2013.01); C10L 2290/547 (2013.01); Y02E 50/30 (2013.01);
Abstract

A method of manufacturing a molded solid fuel including: a pulverization for pulverizing low-grade coal; a mixing for obtaining a slurry by mixing the pulverized low-grade coal and a solvent oil; a dehydration for obtaining a dehydrated slurry by heating and dehydrating the slurry; a solid-liquid separation for obtaining a cake by separating the solvent oil from the dehydrated slurry; a drying for obtaining powdery modified coal by heating the cake and further separating the solvent oil from the cake; and a molding for pressurizing and molding the powdery modified coal by using a molding machine, without the addition/mixture of a binder. In the molding, a coolant is sprayed onto the surface of the molding machine, and the surface temperature of the molding machine is kept equal to or below 100° C.


Find Patent Forward Citations

Loading…