The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 15, 2017

Filed:

May. 14, 2015
Applicant:

Samsung Sdi Co., Ltd., Yongin-si, Gyeonggi-do, KR;

Inventors:

Sang Hee Park, Uiwang-si, KR;

Hyun Jin Koo, Uiwang-si, KR;

Dae Sub Song, Uiwang-si, KR;

Assignee:

SAMSUNG SDI CO., LTD., Yongin-Si, Gyeonggi-Do, KR;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
H01L 21/00 (2006.01); H01B 1/22 (2006.01); H01L 31/0224 (2006.01); C09D 5/24 (2006.01); H01L 31/18 (2006.01); C03C 3/062 (2006.01); C03C 3/07 (2006.01); C03C 3/11 (2006.01); C03C 3/12 (2006.01); C03C 3/16 (2006.01); C03C 3/23 (2006.01); C03C 8/02 (2006.01); C03C 8/08 (2006.01); C03C 8/10 (2006.01); C03C 8/18 (2006.01);
U.S. Cl.
CPC ...
H01B 1/22 (2013.01); C03C 3/062 (2013.01); C03C 3/07 (2013.01); C03C 3/11 (2013.01); C03C 3/122 (2013.01); C03C 3/16 (2013.01); C03C 3/23 (2013.01); C03C 8/02 (2013.01); C03C 8/08 (2013.01); C03C 8/10 (2013.01); C03C 8/18 (2013.01); C09D 5/24 (2013.01); H01L 31/022425 (2013.01); H01L 31/1864 (2013.01); Y02E 10/50 (2013.01);
Abstract

Example embodiments relate to a composition for forming a solar cell electrode, and a solar cell electrode prepared using the composition. The composition for forming a solar cell electrode includes a silver (Ag) powder, a glass frit, and an organic vehicle, wherein the glass frit includes silver (Ag); tellurium (Te); and at least one selected from the group of lithium (Li), sodium (Na), and potassium (K), a molar ratio of the silver (Ag):the tellurium (Te) included in the glass frit is in a range of about 1:0.1 to about 1:50, and a molar ratio of the silver (Ag):lithium (Li), sodium (Na) or potassium (K) is in a range of about 1:0.01 to about 1:10. The solar cell electrode prepared using the composition has excellent fill factor and conversion efficiency due to minimized contact resistance (Rc) and series resistance (Rs).