The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 15, 2017

Filed:

Oct. 14, 2014
Applicant:

Hass Co., Ltd., Gangneung-si, KR;

Inventors:

Yong su Kim, Gangneung-si, KR;

Hyun jun Jeon, Busan, KR;

Hyung bong Lim, Ansan-si, KR;

Kyung sik Oh, Incheon, KR;

Sung ho Ha, Ansan-si, KR;

Jin su Jeong, Donghae-si, KR;

Cheol young Kim, Seoul, KR;

Assignee:

Hass Co., Ltd., Gangneung-si, KR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C03B 19/02 (2006.01); C03B 23/00 (2006.01); C03C 10/00 (2006.01); C03B 32/02 (2006.01); B32B 17/06 (2006.01); C03B 11/08 (2006.01); C03C 3/097 (2006.01); C03C 4/00 (2006.01);
U.S. Cl.
CPC ...
C03C 10/0027 (2013.01); B32B 17/06 (2013.01); C03B 11/08 (2013.01); C03B 19/02 (2013.01); C03B 32/02 (2013.01); C03C 3/097 (2013.01); C03C 4/0021 (2013.01);
Abstract

Exemplary embodiments of the present disclosure provide a lithium silicate crystalline or amorphous glass overlaying the top surfaces of zirconia and the manufacturing process thereof. More specifically, exemplary embodiments of the present disclosure provide a lithium silicate glass or lithium silicate crystalline glass with high light transmittance and good coloring characteristics and the manufacturing process thereof, which overlays the top surface of zirconia with high mechanical strength, frameworks, or copings. The lithium silicate crystalline or amorphous glass may include 10-15 wt % LiO, 71.1-85.0 wt % SiO, 2-5 wt % POworking as nuclear formation agent, 1-5 wt % AlOto increase glass transition temperature and softening temperature, as well as chemical durability of the glass, and 0.01-1.0 wt % ZrOwhich increases the binding strength of the zirconia substructure.