The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 08, 2017

Filed:

Nov. 09, 2012
Applicant:

Nippon Steel & Sumitomo Metal Corporation, Tokyo, JP;

Inventors:

Masahiro Fujikura, Tokyo, JP;

Yoshiyuki Ushigami, Tokyo, JP;

Tesshu Murakawa, Tokyo, JP;

Shinichi Kanao, Tokyo, JP;

Makoto Atake, Tokyo, JP;

Takeru Ichie, Tokyo, JP;

Kojiro Hori, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01F 1/147 (2006.01); C22C 38/00 (2006.01); C22C 38/06 (2006.01); C22C 38/60 (2006.01); H01F 1/16 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C21D 8/02 (2006.01); C21D 8/12 (2006.01);
U.S. Cl.
CPC ...
H01F 1/14775 (2013.01); C21D 8/0263 (2013.01); C21D 8/1222 (2013.01); C21D 8/1233 (2013.01); C21D 8/1272 (2013.01); C22C 38/00 (2013.01); C22C 38/002 (2013.01); C22C 38/004 (2013.01); C22C 38/008 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/60 (2013.01); H01F 1/16 (2013.01); C21D 8/12 (2013.01); C21D 2201/03 (2013.01); H01F 1/14791 (2013.01);
Abstract

A non-oriented electrical steel sheet containing: in mass %, C: 0.005% or less; Si: 0.1% to 2.0%; Mn: 0.05% to 0.6%; P: 0.100% or less; and Al: 0.5% or less, in which 10 pieces/μmor less in number density of non-magnetic precipitate AlN having an average diameter of 10 nm to 200 nm are contained, and an average magnetic flux density B50 in a rolling direction and in a direction perpendicular to rolling is 1.75 T or more. This non-oriented electrical steel sheet can be manufactured by two methods of a method of performing hot rolling annealing at a temperature of 750° C. to an Ac1 transformation point and a method of setting a coil winding temperature to 780° C. or higher and performing self annealing.