The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 01, 2017

Filed:

Feb. 25, 2015
Applicant:

Lincoln Global, Inc., City of Industry, CA (US);

Inventors:

Paul E Denney, Bay Village, OH (US);

Steven R Peters, Huntsburg, OH (US);

David Freeman, South Windsor, CT (US);

Kevin Beardsley, Ashtabula, OH (US);

Assignee:

LINCOLN GLOBAL, INC., City of Industry, CA (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B23K 26/24 (2014.01); B23K 9/02 (2006.01); B23K 9/028 (2006.01); B23K 9/10 (2006.01); B23K 9/23 (2006.01); B23K 26/32 (2014.01); B23K 26/322 (2014.01); B23K 26/211 (2014.01); B23K 26/282 (2014.01); B23K 101/06 (2006.01); B23K 101/10 (2006.01); B23K 101/34 (2006.01); B23K 103/00 (2006.01);
U.S. Cl.
CPC ...
B23K 26/24 (2013.01); B23K 9/0213 (2013.01); B23K 9/0282 (2013.01); B23K 9/1056 (2013.01); B23K 9/1093 (2013.01); B23K 9/23 (2013.01); B23K 26/211 (2015.10); B23K 26/282 (2015.10); B23K 26/32 (2013.01); B23K 26/322 (2013.01); B23K 2201/06 (2013.01); B23K 2201/10 (2013.01); B23K 2201/34 (2013.01); B23K 2203/50 (2015.10);
Abstract

A welding system includes at least one high intensity energy source to create a weld puddle during a root pass on a narrow joint of a workpiece with a clad layer. The system also includes a controller to control a weld ramp out process such that, as the molten puddle advances to a start of an existing root pass weld, the controller at least one of decreases an energy output of the at least one high intensity energy source and reduces an interaction time between the at least one high intensity energy source and the weld puddle. After completion of the root pass, a thickness of a root pass weld in a region that is at or near the start point of the existing root pass weld is in a range of 100 percent to 130 percent of a nominal root pass thickness of a remainder of the root pass weld.