The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 18, 2017

Filed:

Jul. 15, 2014
Applicant:

Exxonmobil Chemical Patents Inc.;

Inventors:

Edward J. Blok, Huffman, TX (US);

Andy H. Tsou, Houston, TX (US);

Shuji Luo, Basking Ridge, NJ (US);

Elizabeth L. Walker, Stockertown, PA (US);

Jingwen Zhang, Houston, TX (US);

Yong Yang, Kingwood, TX (US);

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08F 299/00 (2006.01); C08F 297/00 (2006.01); C08F 299/02 (2006.01); C08L 53/00 (2006.01); B60C 1/00 (2006.01); C08L 9/06 (2006.01); C08C 19/40 (2006.01); C08G 81/02 (2006.01); C08C 19/25 (2006.01); C08C 19/28 (2006.01);
U.S. Cl.
CPC ...
C08F 299/00 (2013.01); B60C 1/0016 (2013.04); C08F 297/00 (2013.01); C08F 299/02 (2013.01); C08L 9/06 (2013.01); C08L 53/00 (2013.01); C08C 19/25 (2013.01); C08C 19/28 (2013.01); C08C 19/40 (2013.01); C08G 81/021 (2013.01);
Abstract

A polyolefin-polybutadiene block-copolymer and a tire tread composition comprising the polyolefin-polybutadiene block-copolymer, the composition comprising, by weight of the composition, within the range from 15 to 60 wt % of a styrenic copolymer, processing oil, filler, a curative agent, and from 4 to 20 wt % of a polyolefin-polybutadiene block-copolymer, wherein the polyolefin-polybutadiene block-copolymer is a block copolymer having the general formula PO-XL-fPB; where 'PO' is a polyolefin block having a weight average molecular weight within the range from 1000 to 150,000 g/mole, the 'fPB' is a functionalized polar polybutadiene block having a weight average molecular weight within the range from 500 to 30,000 g/mole, and “XL” is a cross-linking moiety that covalently links the PO and fPB blocks; and wherein the maximum Energy Loss (Tangent Delta) of the immiscible polyolefin domain is a temperature within the range from −30° C. to 10° C.