The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 11, 2017

Filed:

May. 31, 2013
Applicant:

Lg Chem, Ltd., Seoul, KR;

Inventors:

Joon Koo Kang, Daejeon, KR;

Yeong Rae Chang, Daejeon, KR;

Sung Don Hong, Daejeon, KR;

Soon Hwa Jung, Daejeon, KR;

Eun Kyu Her, Daejeon, KR;

Assignee:

LG CHEM, LTD., Seoul, KR;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C09D 4/00 (2006.01); C08K 3/36 (2006.01); B05D 3/06 (2006.01); C09D 135/02 (2006.01); C09D 133/04 (2006.01); G02B 1/10 (2015.01); C08K 5/3475 (2006.01); C09D 7/12 (2006.01); C09D 105/16 (2006.01); C09D 133/14 (2006.01); C09D 167/00 (2006.01); C08J 7/04 (2006.01); C08J 5/18 (2006.01); C08K 3/22 (2006.01);
U.S. Cl.
CPC ...
C09D 135/02 (2013.01); B05D 3/067 (2013.01); C08J 5/18 (2013.01); C08J 7/04 (2013.01); C08J 7/042 (2013.01); C08J 7/047 (2013.01); C08K 5/3475 (2013.01); C09D 4/00 (2013.01); C09D 7/1216 (2013.01); C09D 7/1241 (2013.01); C09D 105/16 (2013.01); C09D 133/04 (2013.01); C09D 133/14 (2013.01); C09D 167/00 (2013.01); G02B 1/10 (2013.01); G02B 1/105 (2013.01); C08J 2301/12 (2013.01); C08J 2367/02 (2013.01); C08J 2433/14 (2013.01); C08J 2435/02 (2013.01); C08K 3/36 (2013.01); C08K 2003/2227 (2013.01); C08K 2003/2241 (2013.01); C08K 2003/2296 (2013.01); C08K 2201/005 (2013.01); C08K 2201/011 (2013.01); Y10T 428/2495 (2015.01); Y10T 428/259 (2015.01); Y10T 428/269 (2015.01); Y10T 428/31507 (2015.04); Y10T 428/31797 (2015.04); Y10T 428/31884 (2015.04); Y10T 428/31928 (2015.04);
Abstract

A method of preparing a hard coating film by applying a hard coating composition onto both sides of a supporting substrate, thereby forming a hard coating layer on each side of the supporting substrate, the hard coating composition comprising a binder including a tri- to hexa-functional acrylate-based monomer, inorganic particles and a photoinitiator; and irradiating the applied hard coating layers with ultraviolet to simultaneously photocure the hard coating layers, wherein the hard coating film has a pencil hardness of 7H or more under a load of 1 kg, and properties such that when the hard coating film is exposed to a temperature of 50 to 90° C. and a humidity of 80 to 90% for 70 to 100 hours and then placed on a plane, the maximum distance at which each edge of the hard coating film is spaced apart from the plane is 1.0 mm or less.