The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 04, 2017

Filed:

Dec. 11, 2014
Applicant:

Sumitomo Osaka Cement Co., Ltd., Chiyoda-ku, Tokyo, JP;

Inventors:

Takao Kitagawa, Tokyo, JP;

Hirofumi Yasumiishi, Tokyo, JP;

Masaru Uehara, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/131 (2010.01); H01M 4/62 (2006.01); H01M 4/133 (2010.01); H01M 4/485 (2010.01); H01M 4/505 (2010.01); H01M 4/525 (2010.01); C01B 31/02 (2006.01); H01M 4/36 (2006.01); H01M 4/58 (2010.01); H01M 4/02 (2006.01);
U.S. Cl.
CPC ...
H01M 4/625 (2013.01); C01B 31/02 (2013.01); H01M 4/131 (2013.01); H01M 4/133 (2013.01); H01M 4/366 (2013.01); H01M 4/485 (2013.01); H01M 4/505 (2013.01); H01M 4/525 (2013.01); H01M 4/5825 (2013.01); H01M 2004/021 (2013.01); Y02E 60/122 (2013.01); Y02P 70/54 (2015.11);
Abstract

The present invention provides an electrode material in which unevenness in a supporting amount of a carbonaceous film is less when using an electrode-active material having a carbonaceous film on a surface thereof as the electrode material, and which is capable of improving conductivity, and a method for producing the electrode material. The electrode material includes an aggregate formed by aggregating an electrode-active material in which a carbonaceous film is formed on a surface. In the electrode material, an average particle size of the aggregate is 0.5 to 100 μm, a volume density of the aggregate is 50 to 80 vol % of a volume density in a case in which the aggregate is a solid, and 80% or more of the surface of the electrode-active material is covered with the carbonaceous film. Alternatively, the electrode material includes an aggregate formed by aggregating electrode-active material particles in which a carbonaceous film is formed on a surface. In the electrode material, an average particle size of the aggregate is 0.5 to 100 μm, a pore size (D50) when an accumulated volume percentage of a pore size distribution of the aggregate is 50% is 0.1 to 0.2 μm, and porosity of the aggregate is 15 to 50 vol % with respect to a volume in a case in which the aggregate is a solid.


Find Patent Forward Citations