The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 27, 2017

Filed:

Jan. 31, 2012
Applicants:

Yohei Koori, Chiba, JP;

Tomoaki Takebe, Chiba, JP;

Yutaka Minami, Chiba, JP;

Inventors:

Yohei Koori, Chiba, JP;

Tomoaki Takebe, Chiba, JP;

Yutaka Minami, Chiba, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
D01F 1/02 (2006.01); D01F 1/09 (2006.01); D04H 3/16 (2006.01); D04H 3/007 (2012.01); D04H 3/147 (2012.01); D01D 5/098 (2006.01); D01F 1/10 (2006.01); D01F 6/46 (2006.01); C08L 23/02 (2006.01); C08L 91/06 (2006.01); C08L 91/00 (2006.01);
U.S. Cl.
CPC ...
D04H 3/16 (2013.01); D01D 5/0985 (2013.01); D01F 1/10 (2013.01); D01F 6/46 (2013.01); D04H 3/007 (2013.01); D04H 3/147 (2013.01); C08L 23/02 (2013.01); C08L 91/00 (2013.01); C08L 91/06 (2013.01); Y10T 442/681 (2015.04);
Abstract

The method of producing a spunbond nonwoven fabric promotes the bleed out of the additive, which has pleasant texture such as tactile feel and excellent flexibility. The spunbond nonwoven fabric is obtained by this method. Specifically, (1) the method of producing a spunbond nonwoven fabric includes annealing a spunbond nonwoven fabric formed by using a crystalline resin composition (I) containing a low crystalline olefin polymer (a) with an elastic modulus of 10 to 450 MPa in a content of 1 to 50% by mass, a high crystalline olefin polymer (b) with an elastic modulus of 500 to 2,000 MPa, the content of the component (b) being the rest, and an additive (c) in a content of 1 to 20,000 ppm by mass. Furthermore, (2) the method of producing a spunbond nonwoven fabric includes annealing a spunbond nonwoven fabric formed by using a core-sheath composite fiber containing a crystalline resin composition (I) as the sheath component; and a crystalline resin composition (II) as the core component containing a high crystalline olefin polymer (b') with an elastic modulus of 500 to 2,000 MPa.