The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 20, 2017

Filed:

Jun. 17, 2016
Applicant:

Nitto Denko Corporation, Ibaraki-shi, Osaka, JP;

Inventors:

Kenji Furuta, Osaka, JP;

Yoshio Terada, Osaka, JP;

Kota Nakao, Osaka, JP;

Akira Hirao, Osaka, JP;

Ryo Morioka, Osaka, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C09J 7/02 (2006.01); C09J 201/00 (2006.01); B32B 15/08 (2006.01); G11B 33/14 (2006.01); C09J 133/06 (2006.01); C09J 133/08 (2006.01);
U.S. Cl.
CPC ...
C09J 7/0296 (2013.01); B32B 15/08 (2013.01); C09J 7/0246 (2013.01); C09J 133/06 (2013.01); G11B 33/1446 (2013.01); C09J 133/08 (2013.01); C09J 2201/606 (2013.01); C09J 2201/622 (2013.01); C09J 2203/326 (2013.01); C09J 2400/163 (2013.01); C09J 2423/106 (2013.01); C09J 2433/00 (2013.01); C09J 2467/006 (2013.01);
Abstract

A pressure-sensitive adhesive sheet includes a pressure-sensitive adhesive layer and a base including a metal layer and a resin layer, and a product of an initial elastic modulus of the base and a total thickness of the base is 3000 N/mm or less, and a separation distance is 2 mm or less, the separation distance is measured with a peel test with a constant load as follows: a test piece of the pressure-sensitive adhesive sheet having a 10 mm width and a 100 mm length is attached to a surface of a stainless steel test plate and then, the test plate is left standing at a temperature of 23° C. for twenty four hours and then, a load of 100 gf is applied to one end of a length dimension of the test piece vertical to the surface of the test plate and a separation distance of the test piece is measured after one hour.