The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 20, 2017

Filed:

Mar. 18, 2014
Applicants:

Rajen B. Patel, Parsippany, NJ (US);

Victor Stepanov, Highland Park, NJ (US);

Ashok Surapaneni, Hackettstown, NJ (US);

Anthony Distasio, New York, NY (US);

Inventors:

Rajen B. Patel, Parsippany, NJ (US);

Victor Stepanov, Highland Park, NJ (US);

Ashok Surapaneni, Hackettstown, NJ (US);

Anthony DiStasio, New York, NY (US);

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
F42B 33/04 (2006.01); C06B 21/00 (2006.01); C06B 25/34 (2006.01);
U.S. Cl.
CPC ...
C06B 21/0008 (2013.01); C06B 21/0066 (2013.01); C06B 25/34 (2013.01);
Abstract

An effective, safe and economical method of manufacture of an insensitive high explosive molding powder usable as a booster HE. The method preferably involving the steps of adding a binder and a crystalline high explosive to water, grinding that suspension in a bead mill until the crystalline high explosive is nano-sized, and precipitating the binder and crystalline high explosive using a spray dryer. Alternatively, an aqueous suspension of the crystalline high explosive can be ground in the bead mill and the binder subsequently added, prior to spray drying. A fatty alcohol, water defoaming/dispersant/surfactant agent can be added to the dissolved binder/suspended crystalline high explosive, to aid in the manufacturability.