The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 30, 2017

Filed:

Oct. 31, 2012
Applicant:

Yingjin Yuan, Tianjin, CN;

Inventors:

Lianyong Xu, Tianjin, CN;

Hongyang Jing, Tianjin, CN;

Yongdian Han, Tianjin, CN;

Yi Miao, Tianjin, CN;

Assignee:

Tianjin University, Tianjin, CN;

Attorneys:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C21D 9/50 (2006.01); C21D 1/40 (2006.01); H05B 3/14 (2006.01); C21D 9/08 (2006.01); C21D 9/14 (2006.01); C21D 1/30 (2006.01); C21D 1/34 (2006.01); B23K 31/02 (2006.01); H05B 3/34 (2006.01); B23K 101/06 (2006.01); B23K 101/10 (2006.01); B23K 103/04 (2006.01);
U.S. Cl.
CPC ...
C21D 9/50 (2013.01); B23K 31/027 (2013.01); C21D 1/30 (2013.01); C21D 1/34 (2013.01); C21D 1/40 (2013.01); C21D 9/08 (2013.01); C21D 9/14 (2013.01); H05B 3/141 (2013.01); H05B 3/34 (2013.01); B23K 2201/06 (2013.01); B23K 2201/10 (2013.01); B23K 2203/04 (2013.01); C21D 2221/00 (2013.01); Y02B 30/26 (2013.01);
Abstract

The present invention published a large walled field conditions P92 long pipeline local heat treatment processes. Firstly, according to the specific conditions for the on-site grade heat-resistant steel (P92 pipe), combining of the finite element method and test, the Heated Band (HB) width and Gradient Control Band (GCB) was calculated. The pipe was then locally heated using the flexible ceramic resistive heater. When the temperature reaches 80-100° C., the pipe was heated to constant temperature at 80-100° C. for 2 h. The pipe was heated to 300° C. at the rate of 150° C./h. When the temperature reaches 300° C., rising the temperature to 765° C. at the rate of 80° C./h. Holding time is calculated by the wall thickness (5 min/mm, no less than 4 h). Lowering the temperature to 300° C. at the rate of 100° C./h and then natural cooling to room temperature, finally removing the heating device. Finally, the local heat treatment process can be obtained. The present invention can effectively decrease the temperature difference between the outer and inner wall, the residual stress in the welded joints. Thus the service properties can be guaranteed.