The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 09, 2017

Filed:

Sep. 08, 2014
Applicant:

Basf SE, Ludwigshafen, DE;

Inventor:

Matthew D. Wright, Smithfield, VA (US);

Assignee:

BASF SE, Ludwigshafen, DE;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
D21H 21/18 (2006.01); D21H 19/24 (2006.01); C08L 33/26 (2006.01); D21H 17/45 (2006.01); D21H 19/12 (2006.01); D21H 21/20 (2006.01); D21H 23/04 (2006.01); D21H 23/24 (2006.01); D21H 17/55 (2006.01); D21H 17/37 (2006.01); D21H 17/54 (2006.01); D21H 19/20 (2006.01);
U.S. Cl.
CPC ...
D21H 19/24 (2013.01); C08L 33/26 (2013.01); D21H 17/375 (2013.01); D21H 17/45 (2013.01); D21H 17/455 (2013.01); D21H 17/54 (2013.01); D21H 17/55 (2013.01); D21H 19/12 (2013.01); D21H 19/20 (2013.01); D21H 21/18 (2013.01); D21H 21/20 (2013.01); D21H 23/04 (2013.01); D21H 23/24 (2013.01); C08L 2201/54 (2013.01);
Abstract

A cellulose reactive glyoxalated copolymer composition and methods of producing and using the glyoxalated copolymer composition to, for instance, strengthen paper or board are discussed. A glyoxalated copolymer composition includes an aqueous medium containing a glyoxalated copolymer, wherein the glyoxalated copolymer is obtained by reaction in an aqueous reaction medium of a dry weight ratio of glyoxalxationic copolymer. The cationic copolymer can have a weight average molecular weight of about 120,000 to about 1 million Daltons, the cationic copolymer can include diallyldimethylammonium halide monomer and acrylamide monomer, and a ratio a ratio of the weight average molecular weight of the cationic copolymer before glyoxalation to weight % of diallyldimethylammonium halide monomer making up the cationic copolymer before glyoxalation can be equal to or greater than 4,000 or range from 4,000 to 40,000 Daltons/weight %.