The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 09, 2017

Filed:

Feb. 09, 2007
Applicants:

Derek Raybould, Denville, NJ (US);

Thomas E. Strangman, Prescott, AZ (US);

Christian Delacruz, Parsippany, NJ (US);

Inventors:

Derek Raybould, Denville, NJ (US);

Thomas E. Strangman, Prescott, AZ (US);

Christian DelaCruz, Parsippany, NJ (US);

Assignee:

HONEYWELL INTERNATIONAL INC., Morris Plains, NJ (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B05D 3/12 (2006.01); C23C 24/08 (2006.01); C23C 18/04 (2006.01); C23C 18/12 (2006.01); C23C 26/00 (2006.01); F01D 5/28 (2006.01); C23C 28/00 (2006.01);
U.S. Cl.
CPC ...
C23C 24/08 (2013.01); C23C 18/04 (2013.01); C23C 18/1216 (2013.01); C23C 18/1225 (2013.01); C23C 18/1241 (2013.01); C23C 18/1254 (2013.01); C23C 26/00 (2013.01); C23C 28/321 (2013.01); C23C 28/325 (2013.01); C23C 28/345 (2013.01); C23C 28/3455 (2013.01); C23C 28/42 (2013.01); F01D 5/286 (2013.01); F01D 5/288 (2013.01); F05D 2230/90 (2013.01); Y02T 50/67 (2013.01);
Abstract

Exemplary embodiments of the invention provide barrier coated substrates and methods of coating a substrate with a barrier coating derived from sol gels. An example includes a barrier coated aerospace component that is subject to hot salt corrosion during use. The barrier coating is derived from oxidation of a coating composition that includes at least one sol gel. The barrier coating resists hot salt corrosion for an incubation period of such duration that an uncoated superalloy substrate under the same conditions would suffer corrosion to a depth of about 2.0 mils. Methods of applying the barrier coating include the steps of selecting a first liquid sol gel and wetting surfaces of the superalloy substrate with the selected first liquid sol gel. The wetted surfaces of the superalloy substrate are subjected to heat treatment. The heat treatment includes sintering of sol gel to oxide to produce a barrier coating.